Chromium plating anode

Product code: 030004

Product name: chrome bar

Origin: shenzhen hengdi yuan runda industrial co., LTD

Electric discharge oil powder: 40 -- 60g/L

The temperature: 40-58 ℃

Cathode current density: 3 -- 8V/dm2

Or anode electrolysis: 3 -- 8V/dm2

Time: 1-6 minutes

Groove body: PVC or PP plastic board groove inside the groove

Heating: steam iron tube, stainless steel, steel, quartz pen

Anode material:

The package is installed: 25 kg/bag

Sex: basic salt, anionic surfactant, nonionic surfactant

For use: this product is high efficiency, low temperature, weak alkalinity of the electric lifting oil powder, strong ability to remove oil stains, long life, only a small amount of add do not need to replace.Both anode and cathode can be electrolyzed.This product is suitable for steel, copper parts, less oil and chemical or solvent oil removal after the electric oil

 

Origin: Japan

Inches: 45cm, 60cm, 70cm, 80cm, 85cm, 90cm, 100cm

110cm, 120cm, 130cm, 145cm, specific specifications can be customized

Including: 99.99%

Shape: lead-tin alloy has fine grain, good toughness, suitable soft and hard, smooth surface, no sand hole, no defects, no cracks, good polishing and electroplating effect;Lead - tin alloy centrifugal casting performance is good, strong toughness, can cast complex, thin - walled precision parts, casting surface smooth.

Use: lead tin alloy can be used to produce all kinds of exquisite alloy jewelry, alloy crafts, such as rings, necklaces, bracelets, earrings, brooches, buttons, tie clips, hats, craft decorations, alloy photo frames, religious insignia, miniature statues, souvenirs, etc.